Yunsheng Bonded Nd-Fe-B (Compression Moulding)

 

Properties    

 

Grade

Residual

Br mT

(KG)

Coercive

b H c kA/m

(KOe)

Intrinsic Coercive

I H c KA/m

(KOe)

Max. Energy

Product

(BH) max KJ/m3

(MGOe)

Density

D

g/cm3

Reversible permeability

m r

Reversible Thermal

Coefficient

      aBr% /oC

Max. Working temp.

Tw, oC

BNP-6

520-600 (5.2-6.0)

304-360 (3.8-4.5)

640-800 (8.0-10)

40-56 (5-7)

5.3-5.8

1.15

-0.13

140

BNP-8

600-650 (6.0-6.5)

360-440 (4.5-5.5)

640-960 (8.0-12)

56-72 (7-9)

5.6-6.0

1.15

-0.13

140

BNP-10

650-700 (6.5-7.0)

360-464 (4.5-5.8)

640-960 (8.0-12)

72-80 (9-10)

5.8-6.1

1.22

-0.07~-0.105

120

BNP-12

700-760 (7.0-7.6)

424-480 (5.3-6.0)

640-880 (8.0-11)

80-96 (10-12)

6.0-6.2

1.22

-0.13

130

BNP-8H

550-620 (0.5.5-6.2)

400-480 (5.0-6.0)

960-1280 (12-16)

48-72 (6-9)

5.6-6.0

1.15

-0.07~-0.13

120

 

 

Yunsheng Bonded Nd-Fe-B (Injection Moulding)

 

       Properties

 

Grade

Residual

Br mT

(KG)

Coercive

b H c kA/m

(KOe)

Intrinsic Coercive

I H c KA/m

(KOe)

Max. Energy Product

(BH) max KJ/m3

(MGOe)

Density

D

g/cm3

Reversible permeability

m r

Reversible Thermal

Coefficient

 aBr% /oC

BNI-2

200-400 (2.0-4.0)

120-240 (1.5-3.0)

560-720 (7.0-9.0)

6.4-24 (0.8-3.0)

3.5-4.0

1.25

-0.15

BNI-4

400-490 (4.0-4.9)

247-310 (3.1-3.9)

573-732 (7.2-9.2)

28-36 (3.5-4.5)

4.0-5.0

1.20

-0.10

BNI-6

490-570 (4.9-5.7)

312-382 (3.9-4.8)

637-796 (8.0-10.0)

42-56 (5.2-7.0)

5.0-5.5

1.20

-0.10

BNI-8

570-630 (5.7-6.3)

382-430 (4.8-5.4)

676-835 (8.5-10.5)

59-67 (7.4-8.4)

5.0-5.5

1.20

-0.10

BNI-6H

480-560 (4.9-8-5.6)

334-398 (4.2-5.0)

1035-1353 (13.0-17.0)

40-52 (5.0-6.5)

5.0-5.5

1.13

-0.15